ROLLpapercores.infoA ROLL project · ROLL Lab
EN
Find your core
🏆 Your core:

Home › Calculators › The sweating core

Moisture and paper core strength: the calculator

ROLL Lab · app 3 of 11 · Free, full result straight away · updated 24 October 2026

In shortOne extra point of moisture costs about 3.6% of flat crush, 7.1% of radial crush and 12.3% of ID stiffness.
Prof Core

The sweating coreBoard drinks the air. Let’s see how much strength it steals.

radial strength
The core settles at
Flat crush
ID stiffness

ROLL Lab estimate, not a test certificate. Request a test on the real core →

How the calculation works

Board is hygroscopic and reaches equilibrium with the air: most of the way in about a week, the rest over several weeks. The relative humidity → core moisture curve is a rule of thumb widely used in the industry (about 6% moisture at 40% RH, 8% at 55%, about 13% at 80%). The strength losses per point of moisture are ROLL Lab reference data from 7% to 8% on a 3" core with a 13 mm wall.

The ROLL Lab extends these sensitivities with a continuous curve fitted to the trend of flat crush between 4% and 16% moisture. Below 4–5%, paper loses elasticity and turns brittle: drying is not a universal fix.

Sensitivity also depends on the wall: ROLL Lab estimates for a core with a 7.5 mm wall give −20% strength from 8% to 10%. Thin walls can be more sensitive.

Frequently asked questions

How much strength does a paper core lose when it picks up moisture?

According to published studies on a 3" core with a 13 mm wall, one extra point of moisture (from 7% to 8%) costs about 3.6% of flat crush, 7.1% of radial crush and 12.3% of ID stiffness. The calculator "The sweating core" shows the effect at your humidity.

What moisture content should a paper core have?

Usually between 6% and 8%. Below 4–5%, paper turns brittle, because the bonds between fibres need a little water; above 9–10%, strength drops fast. The humidity in the customer’s warehouse matters more than at the production site: the core reaches equilibrium with the air within days.

Why do cores go loose in winter and collapse in summer?

In winter, cold outside air heated indoors has low relative humidity: the core gives off water, shrinks and slips inside the roll. In summer, warm humid air makes the core absorb water and lose radial strength: the inside diameter closes up and the roll gets stuck on the shaft.

Sources

  1. ISO 11093-3 — moisture content by oven drying
  2. ROLL Lab calculation
Want the real number? ROLL Lab estimates help you choose. A specification needs a flat crush and radial crush test on the real core, at the moisture it will work at. Ask for a test or a quote →

The other lab apps